Water Heater Galvanic Corrosion: is electrochemical disintegration that occurs when dissimilar metals come in contact with each other while immersed in an electrolyte. Galvanic corrosion is a major concern anywhere moisture can reach metal building components.

There are 3 conditions need for galvanic corrosion to occur:Water Heater Galvanic Corrosion

  • Two electrochemically dissimilar metals must be in direct contact with each another.
  • There must be an electrically conductive path between the two metals. Any non-metal, liquid substance that can conduct an electric current (such as saltwater or rainwater) can function as an electrolyte.
  • An electrical path must exist to allow metal ions to move from the active metal to the less active metal. (Typically, the metals merely touch one another).

The Statue of Liberty is perhaps the most famous case of galvanic corrosion. Contact between the wrought-iron support and the outer copper skin amidst rainwater exposure has allowed the structure to gradually corrode. The famous icon’s builder anticipated this problem and installed asbestos cloth soaked in shellac insulation in the 1880s.  This worked for some time until it dried up and became porous, acting as a sponge that held saltwater close to the contact points between the two metals. An inspection in 1981 revealed severe galvanic corrosion of the iron supports, causing them to swell and push saddle rivets through the copper skin. This rapidly worsening situation was the main drive to restore the statue in 1986, when the iron was replaced with a variety of corrosion-resistant steel. The solution has held up, and native New Yorkers and visitors alike have been able to enjoy a landmark free from corrosion that will last long into the 21st century.

Examples in Houses

  • ACQ (alkaline copper quaternary) lumber includes copper, which can corrode when it comes in contact with common aluminum building nails. With this type of lumber, it’s best to use G185 galvanized steel or stainless steel fasteners, as they will resist corrosion.
  • Aluminum wiring can become compromised. In the presence of moisture, aluminum will undergo galvanic corrosion when it comes into contact with certain dissimilar metals.
  • Piping commonly rusts and corrodes, especially at joints. The failure of pipe thread is commonly caused by corrosion where carbon steel pipe directly meets a brass valve, or where it transitions to copper pipe. Dielectric unions may be installed to separate these metals to resist damaging corrosion in pipe connections.
  • The elements of an electric water heater often rust and fail. The copper sheathe and steel base, if they become wet, may corrode. Installing galvanized unions with plastic nipples on the top of the water heater can prevent corrosion.

Galvanic Corrosion Can be Prevented in the Following Ways

  • Electrically insulate the dissimilar metals. Plastic can be used to separate steel water pipes from copper-based fittings.  A coat of grease can be used to insulate steel and aluminum parts.
  • Shield the metal from ionic compounds. This is often accomplished by encasing the metal in epoxy or plastic, or painting it. Coating or protection should be applied to the more noble of the two metals, if it is impossible to coat both. Otherwise, greatly accelerated corrosion may occur at points of imperfection in the less noble (more active or anodic) metal.
  • Choose metals that have similar potentials. Closely matched metals have less potential difference and, hence, less galvanic current. The best such solution is to build with only one type of metal.
  • Electroplate the metals.
  • Avoid threaded connections, as they are most severely weakened by galvanic corrosion.
In summary, galvanic corrosion is the disintegration of metals in the presence of an electrolyte. It can occur in homes wherever dissimilar, joined metals become damp.